NEWSLETTER

  • Prepare the substrate

    Prepare the substrate

    The repair process|

    1. Preparing the repair part and its surroundings is a crucial aspect of restoration of …

    Więcej Prepare the substrate
  • Repair Process I

    Repair Process I

    The repair process|

    1. Tools needed for the repair InterTroton or Master silicone remover InterTroton or Master thinner …

    Więcej Repair Process I
  • Repair Process II

    Repair Process II

    The repair process|

    1. Tools needed for the repair InterTroton or Master silicone remover InterTroton or Master thinner …

    Więcej Repair Process II
  • Repair Process III

    Repair Process III

    The repair process|

    1. Tools needed for the repair  InterTroton or Master silicone remover InterTroton or Master thinner …

    Więcej Repair Process III
  • Marking edges (mapping)

    Marking edges (mapping)

    Refinish application defects|

    Cause Incorrect ratio of hardeners and thinners in materials Layers of materials too thick Material …

    Więcej Marking edges (mapping)
  • Pollution in the surface varnish coating

    Pollution in the surface varnish coating

    Refinish application defects|

    Cause Surface to varnish not cleaned properly Dirty paint spray booth Filters in paint spray …

    Więcej Pollution in the surface varnish coating
  • Gasifying

    Gasifying

    Refinish application defects|

    Cause Layers of material too thick Too a short time before drying the material The …

    Więcej Gasifying
  • Loss of adhesion

    Loss of adhesion

    Refinish application defects|

    Cause Lack of recommended thickness for the materials (think, thick) Use of wrong hardeners and …

    Więcej Loss of adhesion
  • Damp patches

    Damp patches

    Refinish application defects|

    Cause Incorrect viscosity of the material Uneven spread of the varnish Too a short time …

    Więcej Damp patches
  • Loss of gloss

    Loss of gloss

    Refinish application defects|

    Cause Lack of recommended thickness for materials (thin, hard) Use of wrong hardeners and thinners …

    Więcej Loss of gloss
  • Orange peel, lack of flow

    Orange peel, lack of flow

    Refinish application defects|

    Cause Too a small nozzle on a spray gun Too high viscosity of varnish Too …

    Więcej Orange peel, lack of flow
  • Crackings on the surface after the repair

    Crackings on the surface after the repair

    Refinish application defects|

    Cause Incorrect gradation of sand paper Bad preparation of the surface for the applied materials …

    Więcej Crackings on the surface after the repair
  • Water stains

    Water stains

    Refinish application defects|

    Cause Wrong ratio of a hardener A distrupted curing process (material not hardened enough) Too …

    Więcej Water stains
  • Blisters

    Blisters

    Refinish application defects|

    Cause Lack of insulation of polyester materials Water condensation when temperature change Polluted installation of …

    Więcej Blisters
  • Discolouration

    Discolouration

    Refinish application defects|

    Cause Bad preparation of the surface to repair Remains of grease from bituminous mass Wrong …

    Więcej Discolouration
  • Ruffle, lifting of a coating

    Ruffle, lifting of a coating

    Refinish application defects|

    Cause Wrong choice of materials (hardeners, thinners) Not properly isolated substrate Thickening of layers of …

    Więcej Ruffle, lifting of a coating
  • Holograms, effects after polishing

    Holograms, effects after polishing

    Refinish application defects|

    Cause Careening of the polishing machine Wrong polishing compound and applicator Too a short time …

    Więcej Holograms, effects after polishing
  • Holes, pinholes

    Holes, pinholes

    Refinish application defects|

    Cause  Too thick layers of polyester putty Airlocked polyester putty , Too a short evaporation …

    Więcej Holes, pinholes
  • Clouds on metallic

    Clouds on metallic

    Refinish application defects|

    Cause Inappropriate viscosity of material Wrong application technique Too dry spray on material Wrong placing …

    Więcej Clouds on metallic
  • No adhesion between a base coat and primer

    No adhesion between a base coat and primer

    Refinish application defects|

    Cause Lack of recommended thickness of materials (thin, thick) Use fine-grained sand paper during primer …

    Więcej No adhesion between a base coat and primer
  • No adhesion between a base coat and a clearcoat

    No adhesion between a base coat and a clearcoat

    Refinish application defects|

    Cause Lack of recommended thickness of materials (thin, thick) Too short evaporation time of base …

    Więcej No adhesion between a base coat and a clearcoat
  • Change of colour shade

    Change of colour shade

    Refinish operating defects|

    Cause Bad quality materials Insufficient amount of UV filters in a product Weather conditions Removal …

    Więcej Change of colour shade
  • Pollution from trees (resin)

    Pollution from trees (resin)

    Refinish operating defects|

    Cause  Aggressive, long lasting tree resin on the surface of the varnish. Countermeasure Regular maintenance …

    Więcej Pollution from trees (resin)
  • Air pollution, precipitation

    Air pollution, precipitation

    Refinish operating defects|

    Cause Polluted rainfall, dust Countermeasure Regular maintenance of the lacquer coating Removal Sand, insulate and …

    Więcej Air pollution, precipitation
  • Stones and sand hitting

    Stones and sand hitting

    Refinish operating defects|

    Cause Damage of the coating especially the front of the vehicle, lower parts (underbody, side …

    Więcej Stones and sand hitting
  • Scratches, damages after using a car wash

    Scratches, damages after using a car wash

    Refinish operating defects|

    Cause Incorrect washing brushes (too hard hair) Wrong choice of the washing program for how …

    Więcej Scratches, damages after using a car wash
  • Bird droppings

    Bird droppings

    Refinish operating defects|

    Cause Aggressive bird droppings in conjunction with a high temperature (the Sun) Not hardened surface …